Tied Universal Expansion Joints for a Chemical Plant in Africa
December 6th, 2002
Comments off
These expansion joints were designed at 170 PSIG and 450 degrees F. to absorb lateral movements and tested per B31.3. They were made with InconelĀ® 625LCF bellows and A105 300 lb. RFSO flanges. The entire assembly was hydro-tested at 255 PSIG and held under pressure for four hours. In order to detect any leaks, each expansion joint and its welds were subjected to the dye penetrant-test and the X-ray test, each of which were 100%, prior to and following forming.